Microstructure and Drying Shrinkage of Cement Mortars Containing High-Volume Fly Ash and Glass Waste Nanoparticles
Résumé fourni par la source
Replacing Ordinary Portland Cement (OPC) with high volumes of fly ash (FA) offers a practical approach to reducing the environmental impacts associated with cement manufacturing and landfill disposal. However, high FA replacement levels, particularly up to 60%, often lead to lower early-age strength. This study developed a green cement mortar containing 60% FA and waste bottle glass nanoparticles (WBGNPs). The WBGNPs were incorporated at replacement levels of 2%, 4%, 6%, 8%, and 10% by volume of the OPC–FA binder. The findings showed that the addition of 4–6% WBGNPs significantly promoted the formation of dense reaction gels and enhanced compressive strength by 12.5–39.1%. Similar performance trends were observed in both the engineering and microstructural properties. The combined incorporation of FA and WBGNPs also improved drying shrinkage performance by reducing capillary stresses during water evaporation and minimizing crack development within the cement matrix. Additionally, a proposed shrinkage prediction model was validated using experimental data and demonstrated good agreement, with an average prediction error of approximately 8%. Overall, the incorporation of WBGNPs provides an effective method for producing high-volume FA cement mortars with satisfactory engineering properties suitable for concrete applications in tropical environments. This approach further supports sustainability by reducing waste generation, lowering landfill demand, and minimizing environmental pollution.